Abstract
Highly luminescent nanocomposites were prepared by incorporating CdSe/CdS core/shell nanorods into different polymer matrices.
The resulting nanocomposites show high transparency of up to 93%. A photoluminescence quantum efficiency of 70% was
obtained, with an optimum combination of nanorod (0.05 wt %) and at a UV-initiator concentration of 0.1 wt % for poly(lauryl
methacrylate). Nanorods tend to agglomerate in cellulose triacetate.